Polymer Property : Impact Test = 74.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 74.0 J

@Temperature -40.0 °C
54.6 ft-lb

@Temperature -40.0 °F
Instrumented Impact Energy @ peak; ASTM D 3763
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Asia Pacific)
Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Asia Pacific region.
Impact Test 74.0 J

@Temperature -40.0 °C
54.6 ft-lb

@Temperature -40.0 °F
Instrumented Impact Energy @ peak; ASTM D 3763
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Europe-Africa-Middle East)
Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.