Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 95.0 J @Thickness 3.17 mm, Temperature -40.0 °C |
70.1 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
ARM Low Temperature Impact on Rotomolded samples; ARM Method |
NOVA Chemicals Surpass® RMs341-U Octene sHDPE Rotational Molding Resin RMs341-U complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. RMs341-.. |
|||
Impact Test | 95.0 J @Thickness 3.17 mm, Temperature -40.0 °C |
70.1 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
ARM Low Temperature Impact on Rotomolded samples; ARM Method |
NOVA Chemicals Surpass® RMs341-UG Octene sHDPE Rotational Molding Resin RMs341-UG complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. RMs341.. |
|||
Impact Test | 95.0 J @Thickness 3.17 mm, Temperature -40.0 °C |
70.1 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
ARM Impact |
Chevron Phillips Marlex® HMN TR-938/938G Polyethylene; MDPE Medium density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: Wide process windows and good flowLong-term UV stabilizationExcellent impact stre.. |