Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 62.2 J @Temperature -30.0 °C |
45.9 ft-lb @Temperature -22.0 °F |
Instrumented Dart Total Energy |
Styron Pulse® 1370 ABS + Polycarbonate PULSE® 1370 Engineering resin offers a superior total performance with a balance of heat resistance, practical toughness, high and low temperature impact strength retention and ease of processing.. |
|||
Impact Test | 62.2 J @Temperature 23.0 °C |
45.9 ft-lb @Temperature 73.4 °F |
Instrumented Dart Total Energy |
Styron Pulse® 1370 ABS + Polycarbonate PULSE® 1370 Engineering resin offers a superior total performance with a balance of heat resistance, practical toughness, high and low temperature impact strength retention and ease of processing.. |
|||
Impact Test | 62.2 J @Temperature -30.0 °C |
45.9 ft-lb @Temperature -22.0 °F |
Instrumented Dart Total Energy |
Styron Pulse® 600 ABS + Polycarbonate PULSE® 600 Engineering resin is designed to offer a superior balance of properties between impact strength, heat resistance and processability. It offers excellent processability, medium heat res.. |
|||
Impact Test | 62.2 J @Temperature -30.0 °C |
45.9 ft-lb @Temperature -22.0 °F |
Instrumented Dart Total Energy |
Styron Pulse® 710 ABS + Polycarbonate PULSE® 710 Engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at both room and low temperatures. PULSE 710 Engineering resin h.. |
|||
Impact Test | 62.2 J @Temperature -30.0 °C |
45.9 ft-lb @Temperature -22.0 °F |
Instrumented Dart Total Energy |
Styron Pulse® 830 ABS + Polycarbonate PULSE® 830 Engineering resin offers excellent processability, high heat resistance, and high impact strength at both room and low temperatures.PULSE 830 Engineering resin has been used in automot.. |