Polymer Property : Impact Test = 5.90 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 8.00 J

@Temperature -30.0 °C
5.90 ft-lb

@Temperature -22.0 °F
Multi-Axial Impact, Fractovis J; Energy Peak; ASTM-D3763
Ineos ABS Lustran® SMA 2171 SMA, Injection Molding Grade
Lustran® SMA 2171 is a high heat injection molding grade of impact-modified SMA (styrene/maleic anhydride) terpolymer offering an exceptional balance of processability and performance. Lustran®..
Impact Test 8.00 J

@Temperature -20.0 °C
5.90 ft-lb

@Temperature -4.00 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Ultem EXUM0169 PEI Blend (Europe-Africa-Middle East)
Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Afri..
Impact Test 8.00 J

@Temperature 23.0 °C
5.90 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Noryl GTX GTX8430W PPE+PA
30% Glass Reinforced PPE+PA Alloy. Typically used for automotive connectors.This data was supplied by SABIC-IP for the Americas region.
Impact Test 8.00 J

@Temperature 23.0 °C
5.90 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics LNP Verton RV004ESV_GY7E070 PA 66
Preliminary data for 20% long glass fiber filled, single pellet color gray, PA66This data was supplied by SABIC-IP for the Americas region.