Polymer Property : Impact Test = 29.2 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 39.5 J

@Temperature -40.0 °C
29.2 ft-lb

@Temperature -40.0 °F
At Break. Deflection: 1359 mils, Failure Mode: Ductile (Instrumented Impact 9000 in/min)
Teknor Apex TELCAR® 1000-92 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Impact Test 39.5 J

@Temperature -40.0 °C
29.2 ft-lb

@Temperature -40.0 °F
At Break. Deflection: 1359 mils, Failure Mode: Ductile (Instrumented Impact 9000 in/min)
Teknor Apex TELCAR® 1000-92UV Thermoplastic Elastomer
Information provided by Teknor Apex Company
Impact Test 39.6 J

@Temperature 23.0 °C
29.2 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Dow AIM® 4810 High Impact Styrenic Resin
AIM® 4810 advanced styrenic resin is designed to offer the processability of high impact polystyrene and the gloss and practical toughness of high gloss ABS. It can be processed at lower temperatur..