Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 28.5 J @Temperature -40.0 °C |
21.0 ft-lb @Temperature -40.0 °F |
Instrumented Impact, Total Energy; ASTM D3763 |
ExxonMobil OPTEMA™ TC 120 Molding Ethylene Methyl Acrylate Product Description: Optema TC 120 is an ethylene methyl acrylate copolymer, which can be used as an impact modifier or compatibilizer in polymer compounds. TC 120 has been processed on typical LDPE.. |
|||
Impact Test | 28.5 J @Temperature 23.0 °C |
21.0 ft-lb @Temperature 73.4 °F |
Instrument Impact, Total Energy; ASTM D3763 |
ExxonMobil ESCOR™ AT 310 Molding, extrusion and compounding resin
(discontinued **) ESCOR AT 310 provides excellent adhesion to a variety of polar and non-polar materials such as metals, glass, polyolefins, polyamides, polyesters, etc. It is suitable for use as a polymer modifier .. |