Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 217 J @Thickness 0.250 mm, Temperature -40.0 °C |
160 ft-lb @Thickness 0.00984 in, Temperature -40.0 °F |
Rotomolded samples; ARM Method |
NOVA Chemicals Novapol® TR-0535-UI Hexene MDPE Rotational Molding Resin TR-0530-UI complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. TR-0530-UI is su.. |
|||
Impact Test | 217 J @Thickness 0.250 mm, Temperature -40.0 °C |
160 ft-lb @Thickness 0.00984 in, Temperature -40.0 °F |
Rotomolded samples; ARM Method |
NOVA Chemicals Novapol® TR-0535-UIG Hexene MDPE Rotational Molding Resin TR-0530-UIG complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. TR-0530-UIG is .. |
|||
Impact Test | 217 J @Thickness 6.35 mm, Temperature -40.0 °C |
160 ft-lb @Thickness 0.250 in, Temperature -40.0 °F |
rotomolded; ARM Method |
NOVA Chemicals Sclair® TD-7915-UG Hexene MDPE Rotational Molding Resin
(discontinued **) Excellent low temperature impact properties, Excellent ESCR, Wide process window, NSF listing for Stds. 14, 24, and 61 pending, Retention of impact at long cook timesApplications: IBCs, Toys, Genera.. |
|||
Impact Test | 217 J @Thickness 6.35 mm, Temperature -40.0 °C |
160 ft-lb @Thickness 0.250 in, Temperature -40.0 °F |
ARM |
ExxonMobil LL 8360.29 Rotational Molding Resin Product Description: LL 8360 is a linear low density hexene copolymer designed to offer excellent processability along with outstanding dimensional control and low warpage. This resin is ideally sui.. |
|||
Impact Test | 217 J @Thickness 6.35 mm, Temperature -40.0 °C |
160 ft-lb @Thickness 0.250 in, Temperature -40.0 °F |
ARM |
ExxonMobil LL 8555.24 Rotational Molding Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
Impact Test | 217 J @Thickness 6.35 mm, Temperature -40.0 °C |
160 ft-lb @Thickness 0.250 in, Temperature -40.0 °F |
ARM |
ExxonMobil LL 8555.25 Rotational Molding Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
Impact Test | 217 J @Thickness 6.35 mm, Temperature -40.0 °C |
160 ft-lb @Thickness 0.250 in, Temperature -40.0 °F |
ARM |
ExxonMobil LLDPE LL 8360.29 Linear Low Density Polyethylene Resin Product Description: LL 8360 is a linear low density hexene copolymer designed to offer excellent processability along with outstanding dimensional control and low warpage. This resin is ideally sui.. |
|||
Impact Test | 217 J @Thickness 6.35 mm, Temperature -40.0 °C |
160 ft-lb @Thickness 0.250 in, Temperature -40.0 °F |
ARM |
ExxonMobil LLDPE LL 8555.24 Linear Low Density Polyethylene Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
Impact Test | 217 J @Thickness 6.35 mm, Temperature -40.0 °C |
160 ft-lb @Thickness 0.250 in, Temperature -40.0 °F |
ARM |
ExxonMobil LLDPE LL 8555.25 Linear Low Density Polyethylene Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
Impact Test | 217 J @Thickness 6.35 mm, Temperature -40.0 °C |
160 ft-lb @Thickness 0.250 in, Temperature -40.0 °F |
ARM |
ExxonMobil LLDPE LLP 8360.29 Linear Low Density Polyethylene Resin Product Description: LL 8360 is a linear low density hexene copolymer designed to offer excellent processability along with outstanding dimensional control and low warpage. This resin is ideally sui.. |
|||
Impact Test | 217 J @Thickness 6.35 mm, Temperature -40.0 °C |
160 ft-lb @Thickness 0.250 in, Temperature -40.0 °F |
ARM |
ExxonMobil LLDPE LLP 8555.24 Linear Low Density Polyethylene Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
Impact Test | 217 J @Thickness 6.35 mm, Temperature -40.0 °C |
160 ft-lb @Thickness 0.250 in, Temperature -40.0 °F |
ARM |
ExxonMobil LLDPE LLP 8555.25 Linear Low Density Polyethylene Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
Impact Test | 217 J @Thickness 6.35 mm, Temperature -40.0 °C |
160 ft-lb @Thickness 0.250 in, Temperature -40.0 °F |
ARM |
ExxonMobil LLP8360.29 Rotational Molding Resin Product Description: LL 8360 is a linear low density hexene copolymer designed to offer excellent processability along with outstanding dimensional control and low warpage. This resin is ideally sui.. |
|||
Impact Test | 217 J @Thickness 6.35 mm, Temperature -40.0 °C |
160 ft-lb @Thickness 0.250 in, Temperature -40.0 °F |
ARM |
ExxonMobil LLP8555.24 Rotational Molding Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
Impact Test | 217 J @Thickness 6.35 mm, Temperature -40.0 °C |
160 ft-lb @Thickness 0.250 in, Temperature -40.0 °F |
ARM |
ExxonMobil LLP8555.25 Rotational Molding Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
Impact Test | 217 J @Thickness 6.35 mm, Temperature -40.0 °C |
160 ft-lb @Thickness 0.250 in, Temperature -40.0 °F |
ARM |
ExxonMobil LL 8360 Rotational Molding Resin
(discontinued **) LL 8360 is a linear low density hexene copolymer designed to provide good processability along with outstanding dimensional control and low warpage. This resin is ideally suited for applications tha.. |
|||
Impact Test | 217 J @Thickness 6.35 mm, Temperature -40.0 °C |
160 ft-lb @Thickness 0.250 in, Temperature -40.0 °F |
ARM |
ExxonMobil LL 8555.67 Rotational Molding Resin
(discontinued **) LL 8555 is a linear low density hexene copolymer designed to offer excellent processability, dimensional control, whiteness and low warpage. This resin is ideally suited for applications that requir.. |
|||
Impact Test | 217 J @Thickness 6.35 mm, Temperature -40.0 °C |
160 ft-lb @Thickness 0.250 in, Temperature -40.0 °F |
rotomolded; ARM Method |
NOVA Chemicals Sclair® TD-7915-U Hexene MDPE Rotational Molding Resin
(discontinued **) Excellent low temperature impact properties, Excellent ESCR, Wide process window, NSF listing for Stds. 14, 24, and 61 pending, Retention of impact at long cook timesApplications: IBCs, Toys, Genera.. |