Mechanical Properties Metric English Comments
Impact Test 203 J

@Thickness 6.35 mm,
Temperature -40.0 °C
150 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
rotomolded; ARM Method
NOVA Chemicals Novapol® TR-0735-U Hexene MDPE Rotational Molding Resin
Good impact resistance, Excellent processabilityApplications: Toys, Complex custom parts, Home and garden items, MailboxesAdditives: Processing antioxidants, UV stabilizersInformation provided by NO..
Impact Test 203 J

@Thickness 6.35 mm
150 ft-lb

@Thickness 0.250 in
ARM Method
NOVA Chemicals Novapol® TR-0735-UG Hexene MDPE Rotational Molding Resin
Features: Good impact properties Excellent processabilityNSF listed for Stds. 14, 24 and 61 Applications: ToysComplex custom partsHome and garden itemsMailboxesInformation provided by Nova Chemicals..
Impact Test 203 J

@Thickness 6.35 mm,
Temperature -40.0 °C
150 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
rotomolded; ARM Method
NOVA Chemicals Sclair® 8107 UV8D Butene LLDPE Rotational Molding Resin
Excellent ESCR, Excellent low temperature impact properties, Excellent low shrinkage and warpage properties, Very good processability, UL 94-HB listedApplications: Food and laundry materials handlin..
Impact Test 203 J

@Thickness 6.35 mm,
Temperature -40.0 °C
150 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
rotomolded; ARM Method
NOVA Chemicals Sclair® 8107G UV8D Butene LLDPE Rotational Molding Resin
Excellent ESCR, Excellent low temperature impact properties, Excellent low shrinkage and warpage properties, Very good processability, UL 94-HB listedApplications: Food and laundry materials handlin..