Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 2.03 J @Temperature 23.0 °C |
1.50 ft-lb @Temperature 73.4 °F |
ASTM D4272 |
ExxonMobil LD331.08 EVA LD 331.08 Very Clear, High Impact Film Resin LD 331 Series films have superior impact strength and heat sealabilityInformation provided by ExxonMobil Chemical |
|||
Impact Test | 2.03 J @Temperature 23.0 °C |
1.50 ft-lb @Temperature 73.4 °F |
ASTM D4272 |
ExxonMobil LD331.99 EVA LD 331.99 Very Clear, High Impact Film Resin LD 331 Series films have superior impact strength and heat sealabilityInformation provided by ExxonMobil Chemical |