Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 2.00 J @Temperature 23.0 °C |
1.48 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics Noryl PX4058 PPE+PS PPO, polyolefin blend. Improved chemical resistance. 253F (125C) HDT.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 2.00 J @Temperature -30.0 °C |
1.48 ft-lb @Temperature -22.0 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics Noryl PX4058 PPE+PS PPO, polyolefin blend. Improved chemical resistance. 253F (125C) HDT.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 2.00 J @Temperature 23.0 °C |
1.48 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics Noryl PX4058 PPE+PS (Asia Pacific) PPO, polyolefin blend. Improved chemical resistance. 253F (125C) HDT.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Impact Test | 2.00 J @Temperature -30.0 °C |
1.48 ft-lb @Temperature -22.0 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics Noryl PX4058 PPE+PS (Asia Pacific) PPO, polyolefin blend. Improved chemical resistance. 253F (125C) HDT.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Impact Test | 2.00 J @Temperature 23.0 °C |
1.48 ft-lb @Temperature 73.4 °F |
Multi-axial, at max. load; ASTM D3763 |
Azdel SuperLite® SL550600-100 PP Resin Matrix / 55% Glass Fiber (2 mm Molded Thickness) AZDEL SuperLite® SL550600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Impact Test | 2.00 J @Temperature 23.0 °C |
1.48 ft-lb @Temperature 73.4 °F |
Multi-axial, at max. load; ASTM D3763 |
Azdel SuperLite® SL550600-100 PP Resin Matrix / 55% Glass Fiber (2.5 mm Molded Thickness) AZDEL SuperLite® SL550600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Impact Test | 2.00 J @Temperature 23.0 °C |
1.48 ft-lb @Temperature 73.4 °F |
Multi-axial, at max. load; ASTM D3763 |
Azdel SuperLite® SL550600-100 PP Resin Matrix / 55% Glass Fiber (3.5 mm Molded Thickness) AZDEL SuperLite® SL550600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Impact Test | 2.00 J @Temperature 23.0 °C |
1.48 ft-lb @Temperature 73.4 °F |
Multi-axial, at max. load; ASTM D3763 |
Azdel SuperLite® SL550700-100 PP Resin Matrix / 55% Glass Fiber (2.5 mm Molded Thickness) AZDEL SuperLite® SL550700-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Impact Test | 2.00 J @Temperature 23.0 °C |
1.48 ft-lb @Temperature 73.4 °F |
Multi-axial, at max. load; ASTM D3763 |
Azdel SuperLite® SL550700-100 PP Resin Matrix / 55% Glass Fiber (3.5 mm Molded Thickness) AZDEL SuperLite® SL550700-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Impact Test | 2.00 J @Temperature 23.0 °C |
1.48 ft-lb @Temperature 73.4 °F |
Multi-axial, at max. load; ASTM D3763 |
Azdel SuperLite® SL550800-100 PP Resin Matrix / 55% Glass Fiber (1.5 mm Molded Thickness) AZDEL SuperLite® SL550800-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |