Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Impact Test = 19.9 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 27.0 J

@Thickness 3.17 mm,
Temperature -40.0 °C
19.9 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
Rotational Molded, Instrumented
NOVA Chemicals Surpass® RMs539-U Octene sMDPE Rotational Molding Film
Features: Octene copolymerExceptional low temperature impact propertiesOutstanding stiffnessBroad processing windowSuperior whiteness for improved part appearanceEasy mold releaseNSF listed for Stan..
Impact Test 27.0 J

@Thickness 3.17 mm,
Temperature -40.0 °C
19.9 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
Rotational Molded, Instrumented
NOVA Chemicals Surpass® RMs539-UG Octene sMDPE Rotational Molding Film
Features: Octene copolymerExceptional low temperature impact propertiesOutstanding stiffnessBroad processing windowSuperior whiteness for improved part appearanceEasy mold releaseNSF listed for Stan..
Impact Test 27.0 J

@Temperature -30.0 °C
19.9 ft-lb

@Temperature -22.0 °F
Instrumented Impact Energy @ peak; ASTM D 3763
SABIC Innovative Plastics Noryl GTX GTX917 PPE+PS+PA
This data was supplied by SABIC-IP for the Americas region.
Impact Test 27.0 J

@Temperature -18.0 °C
19.9 ft-lb

@Temperature -0.400 °F
ASTM D3763
Diamond Polymers Centrex® 825 Sheet Extrusion Grade
Centrex 825 resin is a high-gloss, high-impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, and it ..
Impact Test 27.0 J

@Temperature 23.0 °C
19.9 ft-lb

@Temperature 73.4 °F
Total Energy; ASTM D3763
Diamond Polymers DIAMALOY GLY 7510 High Heat ASA Weatherable Polymer
Diamaloy GLY 7510 resin is a high gloss, high heat and high impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. This product is rated f1 by UL and be customed..
Copyright © lookpolymers.com All Rights Reserved