Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 237 J @Thickness 6.35 mm, Temperature -40.0 °C |
175 ft-lb @Thickness 0.250 in, Temperature -40.0 °F |
ARM Impact |
Chevron Phillips Marlex® HMN TR-935/935G Polyethylene; MDPE Medium density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: Wide process windows and excellent flowLong-term UV stabilizationExcellent impac.. |
|||
Impact Test | 237 J @Thickness 6.35 mm, Temperature -40.0 °C |
175 ft-lb @Thickness 0.250 in, Temperature -40.0 °F |
ARM Impact |
Chevron Phillips Marlex® HMN TR-938/938G Polyethylene; MDPE Medium density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: Wide process windows and good flowLong-term UV stabilizationExcellent impact stre.. |