Polymer Property : Impact Test = 16.7 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test >= 22.6 J

@Thickness 5.99 mm,
Temperature 22.8 °C
>= 16.7 ft-lb

@Thickness 0.236 in,
Temperature 73.0 °F
Drop Ball Impact Test, 1 inch dart
Plaskolite Mustang PETG Sheet
MUSTANG sheet signage material is continually processed using Eastman Tritan® copolyester, MUSTANG offers superior forming details, improved material distribution and shorter heating and cooling cy..
Impact Test >= 22.6 J

@Thickness 5.99 mm,
Temperature -17.8 °C
>= 16.7 ft-lb

@Thickness 0.236 in,
Temperature 0.000 °F
Drop Ball Impact Test, 1 inch dart
Plaskolite Mustang PETG Sheet
MUSTANG sheet signage material is continually processed using Eastman Tritan® copolyester, MUSTANG offers superior forming details, improved material distribution and shorter heating and cooling cy..
Impact Test 22.6 J

@Temperature -40.0 °C
16.7 ft-lb

@Temperature -40.0 °F
At Yield. Deflection: 693 mils, Force: 425 lbs (Instrumented Impact, 9000 in/min)
Teknor Apex TELCAR® 1000-92 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Impact Test 22.6 J

@Temperature -40.0 °C
16.7 ft-lb

@Temperature -40.0 °F
At Yield. Deflection: 693 mils, Force: 425 lbs (Instrumented Impact, 9000 in/min)
Teknor Apex TELCAR® 1000-92UV Thermoplastic Elastomer
Information provided by Teknor Apex Company