Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact Unnotched | 32.5 - 42.0 J | 24.0 - 31.0 ft-lb | |
Carpenter Micro-Melt® M-3 Class 2 Alloy (AISI M3) Micro-Melt® M-3 Class 2 alloy is a powder metal tungsten-molybdenum high-speed steel possessing the superior wear resistance characteristics required for difficult cutting operations. The advantage.. |