Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Strength = 98.94 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 98.94 MPa
14350 psi
ASTM D695
Ensinger TECASON™ P MT Polyphenylsulfone (PPSU)
TECASON™ P MT is a polyphenylsulfone suited primarily to applications in the medical industry. It has improved performance in terms of temperature, impact strength and chemical resistance, as well..
Compressive Strength 98.94 MPa
14350 psi
ASTM D695
Ensinger TECASON™ P Polyphenylsulfone (PPSU)
TECASON™ P is a polyphenylsulfone that exhibits excellent temperature, impact and chemical resistance properties.
Compressive Strength 98.94 MPa
14350 psi
ASTM D695
Ensinger RADEL® R-5500 Polyphenylsulfone (PPSU)
RADEL® R is a Polyphenysulfone produced by Solvay Advanced Polymers. RADEL® R is in the same performance category as products like Polysulfone and ULTEM® (PEI). RADEL® R has increased performa..