Polymer Property : Compressive Strength = 91.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 91.0 MPa
13200 psi
10% Def.; ASTM D695
Quadrant EPP Acetron® MD Metal-detectable Copolymer Acetal (ASTM Product Data Sheet)
Low moisture absorption High strength, stiffness Easy to machine No centerline porosity in Acetron® GP Many formulation options: Copolymer, Homopolymer, PTFE filled, and Internally lubricated/enha..
Compressive Strength 91.0 MPa
13200 psi
10% Def.; ASTM D695
Quadrant EPP PPO Polyphenylene oxide, unfilled, extruded (ASTM Product Data Sheet)
Data provided by Quadrant Engineering Plastic Products.
Compressive Strength 91.0 MPa
13200 psi
20% pressing; EN ISO 604
Schwartz Technical Plastics LAMIGAMID® 317 Cast Polyamide 6, Heat Stabilized, Conditioned
Application: coupling parts, sealing rings, bearingsInformation provided by Schwartz Technical Plastics GmbH
Compressive Strength 91.0 MPa
13200 psi
20% pressing; EN ISO 604
Schwartz Technical Plastics LAMIGAMID® 317 Cast Polyamide 6, Heat Stabilized, Dry
Application: coupling parts, sealing rings, bearingsInformation provided by Schwartz Technical Plastics GmbH
Compressive Strength 91.0 MPa
13200 psi
20% pressing; EN ISO 604
Schwartz Technical Plastics LAMIGAMID® 324 Cast Polyamide 6, MoS2, Heat Stabilized, Conditioned
Application: heavy-duty wheels, running speed up to 3m/sInformation provided by Schwartz Technical Plastics GmbH
Compressive Strength 91.0 MPa
13200 psi
20% pressing; EN ISO 604
Schwartz Technical Plastics LAMIGAMID® 324 Cast Polyamide 6, MoS2, Heat Stabilized, Dry
Application: heavy-duty wheels, running speed up to 3m/sInformation provided by Schwartz Technical Plastics GmbH
Compressive Strength 91.0 MPa
13200 psi
20% pressing; EN ISO 604
Schwartz Technical Plastics LAMIGAMID® 327 Cast Polyamide 6, MoS2, Heat Stabilized, Conditioned
Application: heavy-duty wheels, running speed up to 3m/sInformation provided by Schwartz Technical Plastics GmbH
Compressive Strength 91.0 MPa
13200 psi
20% pressing; EN ISO 604
Schwartz Technical Plastics LAMIGAMID® 327 Cast Polyamide 6, MoS2, Heat Stabilized, Dry
Application: heavy-duty wheels, running speed up to 3m/sInformation provided by Schwartz Technical Plastics GmbH
Compressive Strength 91.0 MPa
13200 psi
BCC Products Kwik Kast BC 8001 Urethane Casting
BC8001 is an advanced fast cast polyurethane tooling system. It features low viscosity, low exotherm and minimal shrinkage. It cures hard, yet more durable resulting in less brittle parts. Designed..