Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 620 MPa @Treatment Temp. 50.0 °C, Time 3600 sec |
89900 psi @Treatment Temp. 122 °F, Time 1.00 hour |
ISO 604; IEC/EN 60893-2 5.3 |
Elektro-Isola G-Etronax B Phenolic, Glass Fabric Reinforcement, Dark Brown, Sheet High performance/price ratio insulation material. Self-extinguishing, halogen-free, very low smoke emission and toxicity. Mechanically much stronger than the Etronit and Etronax types.Information pr.. |
|||
Compressive Strength | >= 620 MPa | >= 89900 psi | Ambient |
China-Yixing Longly Refractories ZTA (10%ZrO2) Zirconia Toughened Alumina Composite Ceramic LONGLY's Zirconia Toughened Alumina ceramics (hereafter referred as composite ceramic, ZTA) is white, corrosion resistance, good chemical stability. As well all know that alumina is hard, while zir.. |