Mechanical Properties Metric English Comments
Compressive Strength 41.0 MPa
5950 psi
across grain
Pyrotek PT-10 Graphite
PT-10 Graphite offers the highest resistance to oxidation available. Its unique composition gives it the most durable, long lasting, oxidation resistant properties available from treated graphite.A..
Compressive Strength 41.0 MPa
5950 psi
Pyrotek Pyrocast ICL Castable Refractory
Pyrocast ICL was developed exclusively for the induction furnace market as a coil lining refractory. This silica and alumina based material displays high strength and excellent thermal shock resist..
Compressive Strength 41.0 MPa
5950 psi
Du-Co Ceramics DC-142 Aluminum Silicate
Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company.
Compressive Strength 41.0 - 58.0 MPa
5950 - 8410 psi
ASTM D695
Arkema Group KYNAR FLEX® 2850 Black Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Compressive Strength 41.0 - 58.0 MPa
5950 - 8410 psi
ASTM D695
Arkema Group KYNAR FLEX® 2850-02 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Compressive Strength 41.0 - 58.0 MPa
5950 - 8410 psi
ASTM D695
Arkema Group KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Compressive Strength 41.0 - 58.0 MPa
5950 - 8410 psi
ASTM D695
Arkema Group KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Compressive Strength 41.0 - 58.0 MPa
5950 - 8410 psi
ASTM D695
Arkema Group KYNAR FLEX® 2850-07 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..