Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 530 MPa @Treatment Temp. 100 °C, Time 3600 sec |
76900 psi @Treatment Temp. 212 °F, Time 1.00 hour |
ISO 604; IEC/EN 60893-2 5.3 |
Elektro-Isola G-Etronax B Phenolic, Glass Fabric Reinforcement, Dark Brown, Sheet High performance/price ratio insulation material. Self-extinguishing, halogen-free, very low smoke emission and toxicity. Mechanically much stronger than the Etronit and Etronax types.Information pr.. |
|||
Compressive Strength | 530 MPa @Treatment Temp. 50.0 °C, Time 3600 sec |
76900 psi @Treatment Temp. 122 °F, Time 1.00 hour |
ISO 604; IEC/EN 60893-2 5.3 |
Elektro-Isola G-Etronax EP 11 Epoxy, Glass Fabric Reinforcement, Green, Sheets Description: High resistance to chemicals. Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic t.. |