Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 0.345 - 10.3 MPa | 50.0 - 1500 psi | |
Monmouth Rubber & Plastics Bondaflexâ„¢ B33CS Sponge Neoprene Blend Information provided by Monmouth Rubber & Plastics Corp. |
|||
Compressive Strength | 0.345 MPa | 50.0 psi | 10% Deformation; Green |
Unifrax Fiberfrax® Duraboard® LD Ceramic Fiber Board Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard .. |
|||
Compressive Strength | 0.345 MPa | 50.0 psi | 25% Compression, Deflection |
3M Cushion-Mount™ E1715 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Compressive Strength | 0.345 MPa | 50.0 psi | 25% Compression, Deflection |
3M Cushion-Mount™ 1720M Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Compressive Strength | 0.345 MPa | 50.0 psi | 25% Compression, Deflection |
3M Cushion-Mount™ E1720 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |