Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 430 MPa @Treatment Temp. 200 °C, Time 3600 sec |
62400 psi @Treatment Temp. 392 °F, Time 1.00 hour |
ISO 604; IEC/EN 60893-2 5.3 |
Elektro-Isola G-Etronax B Phenolic, Glass Fabric Reinforcement, Dark Brown, Sheet High performance/price ratio insulation material. Self-extinguishing, halogen-free, very low smoke emission and toxicity. Mechanically much stronger than the Etronit and Etronax types.Information pr.. |
|||
Compressive Strength | >= 430 MPa | >= 62400 psi | Ambient |
China-Yixing Longly Refractories Tube SiC SiC tube made by our company have lots of superior performance, such as high refractoriness, good wear and corrosion resistance, hardness, strength, thermal conductivity, thermal shock stability, as.. |