Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Strength = 37000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 255 MPa
37000 psi
10% Def.; ASTM D695
Quadrant EPP Duratron® T7130 PAI Polyamide-imide, carbon fiber reinforced, extruded (ASTM Product Data Sheet)
Compressive Strength 255 MPa
37000 psi
CE Phenolic Laminate
Cotton based phenolic provides more mechanical strength than paper grades and has a finer surface with better machinability. This material is used for gears, pinions, bearings, bushings, and many s..
Compressive Strength 255 MPa
37000 psi
Haysite H-193 Corrosion Resistant Polyester/Glass Sheet
A fiber glass reinforced thermoset polyester sheet having good corrosion resistance to numerous acids and alkalis. This material also exhibits a high level of flame retardancy and low smoke generati..
Compressive Strength 255 MPa
37000 psi
ASTM D695
Greene Tweed Orthetek® RP Polyketone, Random Carbon Fiber
Greene Tweed offers precision-molded thermoplastic components made form out high-performance Orthtek® composite materials for a variety of demanding medical device applications. Orthtek RP is id..
Compressive Strength 255 MPa
37000 psi
ASTM D695
Solvay Specialty Polymers Ryton® BR42B Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® BR42B 40% glass fiber reinforced polyphenylene sulfide compound is specially formulated to provide low coefficient of friction and reduced wear rate for use in applications requiring low s..
Compressive Strength 255 MPa
37000 psi
ASTM D695
Solvay Specialty Polymers Ryton® XK2340 Polyphenylene Sulfide Alloy (PPS Alloy), 40% Glass Fiber
Ryton® XK2340 40% glass fiber reinforced polyphenylene sulfide alloy compound provides excellent mechanical strength, toughness, and rigidity, along with excellent flow in thin-walled parts, low ..
Compressive Strength 255 MPa
37000 psi
ASTM D695
Sumitomo Bakelite North America EM 7302 Hardware Grade Epoxy
Long fiberglass reinforced epoxy molding compound which features high strength and toughness for structural components. This compound is designed for applications requiring Mil-M-46069 certificatio..
Compressive Strength 255 MPa

@Temperature 23.0 °C
37000 psi

@Temperature 73.4 °F
EN ISO 604
Ensinger TECASINT™ 2022 Polyimide, Black, 15% Graphite (PI)
TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications...
Compressive Strength 255 MPa
37000 psi
Pyrotek TS-81 Thermoset Electrical Insulation Product (Nema Grade: CE)
Cotton reinforcement, Phenolic resin, Natural / Tan color. Economy grade. Good acid resistance.ApplicationsSuperstructure support pads Bus bar insulators Pot cradle insulators Exhaust duct insulat..
Compressive Strength 255 MPa
37000 psi
ASTM D695
Sumitomo Bakelite North America FM 4005 Fiberglass Reinforced Phenolic Novolac
FM 4005 is a fiberglass reinforced phenolic novolac molding compound, with excellent dimensional stability and good strength at elevated temperatures. This material is compliant with the specificat..
Copyright © lookpolymers.com All Rights Reserved