Polymer Property : Compressive Strength = 35400 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 244 MPa
35400 psi
SABIC Method
SABIC Innovative Plastics LNP THERMOCOMP EC006PXQ PEI
LNP* THERMOCOMP* EC006PXQ is a compound based on Polyetherimide containing 30% Carbon FIber. Added features include: Electrically Conductive, Easy Molding.
Compressive Strength 244 MPa
35400 psi
Abatron AboCast 8501-6 One-Component Epoxy
AboCast 8501-6 is a clear, high-temperature one-component epoxy system for very high-temperature uses. It offers the highest heat resistance of the clear resins. Suggested Uses: Casting; Potting; E..