Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 211 MPa @Temperature 204 °C |
30600 psi @Temperature 400 °F |
ASTM D695 |
Haysite H330 Polyester Composite A thermoset polyester composite that offers superior energy efficiency, temperature control, and durability for high temperature mold and platen thermal applications. A proven, cost effective produ.. |
|||
Compressive Strength | 211 MPa @Temperature 23.0 °C |
30600 psi @Temperature 73.4 °F |
EN ISO 604 |
Ensinger TECASINT 1611 Polyimide, 30% PTFE Filled (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |