Mechanical Properties Metric English Comments
Compressive Strength 3.40 MPa
493 psi
to 30% deformation with density of 0.352 g/cc
Pyrotek MT-29B Microporous Insulating Board
MT-29B has the low thermal conductivity. Its cellular structure contributes to its low-weight, good compressive strength, and low shrinkage at high temperatures.ApplicationsBackup insulation for: T..