Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 2.00 MPa | 290 psi | EN 1094-5: 1995 |
Skamol Group ISOPERLOR 550P Perlite Insulating Brick & Block ISOPERLOR perlite insulating bricks & blocks have the following characteristics: Max. service temperature 900°C (1652°F)Back-up insulation onlyExcellent insulating propertiesVery lightweight a.. |
|||
Compressive Strength | 2.00 MPa | 290 psi | Cold |
Unifrax Excelfrax® 1900 Panel Microporous Insulation Unifrax Corporation's Excelfrax® product line, based on advanced microporous insulation technology, is a family of products which all exhibit superior insulating characteristics. Excelfrax micropo.. |
|||
Compressive Strength | 2.00 MPa | 290 psi | Lower Yield in the Through Plane Direction |
Cymat A35620SC 040SS Stabilized Aluminum Foam Description: Cymat A35620SC 040SS stabilized aluminum foam (SAF) is a closed cell aluminum foam formed from A356 aluminum alloy with a density of 0.4 g/cm3. The mechanical properties of SAF make it .. |
|||
Compressive Strength | 2.00 MPa | 290 psi | Cold Crush Strength; ASTM C133 |
BNZ Materials BNZ-26-60 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Compressive Strength | 2.00 MPa | 290 psi | Cold Crush Strength; ASTM C133 |
BNZ Materials BNZP-23 Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Compressive Strength | 2.00 MPa | 290 psi | Cold Crush Strength; ASTM C133 |
BNZ Materials BNZP-23B Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Compressive Strength | 2.00 MPa | 290 psi | Cold Crush Strength; ASTM C133 |
BNZ Materials BNZP-25L Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Compressive Strength | 2.00 MPa @Temperature 200 °C |
290 psi @Temperature 392 °F |
ISO 604 |
Brandenburger BL 70 Slide Bearing Material BL 70 is a low friction material that exhibits stability at high temperatures. Its applications include high-load low friction tracks and linings in transport and conveying systems, high-stressed b.. |
|||
Compressive Strength | 2.00 MPa | 290 psi | average; perpendicular to plane; ISO 844 |
3A Composites Core Materials AIREX® C70.90 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible .. |
|||
Compressive Strength | 2.00 MPa | 290 psi | average; perpendicular to plane; ISO 844 |
3A Composites Core Materials AIREX® T90.150 Easy Processing Structural FST Foam AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has very good mechanical properties and a good resistance to fatigu.. |