Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 24.5 - 29.4 MPa | 3560 - 4270 psi | Cold Crushing |
Sharadaa Ceramics HH 42D Normal Medium and High Heat and Super Duty Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Compressive Strength | 19.6 - 29.4 MPa @Temperature 1500 °C, Time 10800 sec |
2840 - 4270 psi @Temperature 2730 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories TAST-170 Monolithic Refractories for Ladle and Tundish Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |