Polymer Property : Compressive Strength = 2800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 19.3 MPa
2800 psi
10% Def.; ASTM D695
Quadrant EPP Durapro® Truck Liners (ASTM Product Data Sheet)
Compressive Strength 19.3 MPa
2800 psi
10% Def.; ASTM D695
Quadrant EPP TIVAR® 88 W/BurnGuard, Flame Retardant Lining Material (ASTM Product Data Sheet)
Promotes reliable, steady bulk material flow Abrasion-, chemical- and corrosion-resistant Low coefficient of friction No moisture absorption Reduces or eliminates arching, ratholing and erractic fl..
Compressive Strength 19.3 MPa
2800 psi
10% Def.; ASTM D695
Quadrant EPP TIVAR® ECO UHMW-PE, Recycled (ASTM Product Data Sheet)
Compressive Strength 19.3 MPa
2800 psi
ASTM D-695
CMT Materials REN Shape® 450 Prototype Tool & Modeling Board
REN Shape 450 is the preferred modeling board for pattern makers throughout the world. The outstanding dimensional stability and its ability to hold precise tolerances even after exposure to heat h..