Mechanical Properties Metric English Comments
Compressive Strength 190 - 280 MPa
27600 - 40600 psi
Goodfellow Potassium Aluminosilicate (Muscovite Mica)
Mica is a naturally occurring mineral and as such its exact composition varies between grades, as will its properties. Ruby Mica is the highest grade of Muscovite Mica. The name comes from the Latin..
Compressive Strength 240 - 280 MPa
34800 - 40600 psi
ISO 604
Vyncolit X682 Novolac Phenolic
Glass fiber, glass bead and graphite filled phenolic molding compound with excellent mechanical properties and a low coefficient of friction.USES: Water pump seals and self-lubricating bearings.Info..