Polymer Property : Compressive Strength = 24.5 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 24.5 MPa
3550 psi
19%, 0.44 w/c w/Tychem 3000
Mallard Creek Polymers Tychem® 3100D Yield Modifier Additive
Tychem® 3000/3100D is well suited, but not limited to, dry-cast pavers and blocks, SCC, HPC, pre-cast and down hole cementing. Tychem® 3000/3100D is compatible under the most extreme condition..
Compressive Strength 24.5 MPa
3560 psi
Cold Crushing
Sharadaa Ceramics HH 40D Normal Medium and High Heat and Super Duty Brick
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..
Compressive Strength 24.5 - 29.4 MPa
3560 - 4270 psi
Cold Crushing
Sharadaa Ceramics HH 42D Normal Medium and High Heat and Super Duty Brick
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..
Compressive Strength 24.5 MPa
3560 psi
Cold Crushing
Sharadaa Ceramics MH 30D Normal Medium and High Heat and Super Duty Brick
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..
Compressive Strength 24.5 MPa
3560 psi
Fired at 400°C, Cold Crushing
Sharadaa Ceramics REFINSUL ZAP-021 Insulating Castables
Description: We provide our clients a range of Insulating Castables, that are used as backup layer in process industries and hot face layer in petrochemical industry. These castables are known for l..
Compressive Strength <= 24.5 MPa
<= 3560 psi
Cold Crushing Strength
Chosun Refractories BPR-DS Gas Purging Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 24.5 MPa
3560 psi
Cold Crushing Strength
Chosun Refractories CRAG-L38 Shroud Nozzle
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).