Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Strength = 2320 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 16.0 MPa
2320 psi
1% strain over 1000 hours; ISO.899 DIN.53444
Omnia Plastica Noryl® PPO m Polyphenylenoxide
Noryl is a resin based on polyphenylene oxide, modified with styrene. Its main field of application is the electrical one.Features:Good electrical properties, even at high frequency Dimensional stab..
Compressive Strength 16.0 MPa
2320 psi
Pyrotek Pyrite N-17 Refractory Board
Pyrotek N-17 is a graphite fiber reinforced, high purity, calcium silicate board developed exclusively for the non-ferrous casting industry. The patented formulation of Pyrotek N-17 makes it good i..
Compressive Strength 16.0 MPa
2320 psi
5% pressing; EN ISO 604
Schwartz Technical Plastics LAMIGAMID® 700 Ultra High Molecular Weight Polyethylene
Application: wear liners, sliding platesInformation provided by Schwartz Technical Plastics GmbH
Compressive Strength 16.0 MPa
2320 psi
Elastic Limit
Wolf Kunststoff ZEDEX® ZX-550 A5L Polymer Alloy
Main Characteristics: Strong anti-adhesive; Low creep; Weather resistant; No water absorption; Good machinability; Strongly viscoelastic; Stress resistantApplications: Chemical Engineering; Laborato..
Compressive Strength 16.0 MPa

@Strain 3.50 %
2320 psi

@Strain 3.50 %
DIN EN ISO 604
Wolf Kunststoff ZEDEX® ZX-550 A5L Polymer Alloy
Main Characteristics: Strong anti-adhesive; Low creep; Weather resistant; No water absorption; Good machinability; Strongly viscoelastic; Stress resistantApplications: Chemical Engineering; Laborato..
Compressive Strength >= 16.0 MPa
>= 2320 psi
Beijing Evergrow Resources PTFE, 15% Carbon Fiber Filled
Filled PTFE article is manufactured by molding method with filled PTFE resin. Filled PTFE resin is manufactured by compounding PTFE granular resin with fillers of many different kinds. Amongst the m..
Compressive Strength >= 16.0 MPa
>= 2320 psi
Beijing Evergrow Resources PTFE, 20% Glass Fiber Filled
Filled PTFE article is manufactured by molding method with filled PTFE resin. Filled PTFE resin is manufactured by compounding PTFE granular resin with fillers of many different kinds. Amongst the m..
Compressive Strength >= 16.0 MPa
>= 2320 psi
Beijing Evergrow Resources PTFE, 20% Glass Fiber, 5% Graphite Filled
Filled PTFE article is manufactured by molding method with filled PTFE resin. Filled PTFE resin is manufactured by compounding PTFE granular resin with fillers of many different kinds. Broadly speak..
Compressive Strength >= 16.0 MPa
>= 2320 psi
Beijing Evergrow Resources PTFE, 24% Bronze, 12% Glass Fiber, 6% Graphite Filled
Filled PTFE article is manufactured by molding method with filled PTFE resin. Filled PTFE resin is manufactured by compounding PTFE granular resin with filler. Broadly speaking PTFE compounds have t..
Compressive Strength >= 16.0 MPa
>= 2320 psi
Beijing Evergrow Resources PTFE, 25% Glass Fiber Filled
Filled PTFE article is manufactured by molding method with filled PTFE resin. Filled PTFE resin is manufactured by compounding PTFE granular resin with filler. Broadly speaking PTFE compounds have t..
Copyright © lookpolymers.com All Rights Reserved