Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 2.45 MPa | 356 psi | Fired at 800°C, Cold Crushing |
Sharadaa Ceramics REFINSUL ZAP-017 Insulating Castables Description: We provide our clients a range of Insulating Castables, that are used as backup layer in process industries and hot face layer in petrochemical industry. These castables are known for l.. |
|||
Compressive Strength | 2.45 MPa | 356 psi | Dried at 110°C, Cold Crushing |
Sharadaa Ceramics REFINSUL ZAP-015 Insulating Castables Description: We provide our clients a range of Insulating Castables, that are used as backup layer in process industries and hot face layer in petrochemical industry. These castables are known for l.. |
|||
Compressive Strength | <= 2.45 MPa | <= 356 psi | Cold Crushing Strength |
Chosun Refractories B-1 Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | <= 2.45 MPa | <= 356 psi | Cold Crushing Strength |
Chosun Refractories B-2 Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | <= 2.45 MPa | <= 356 psi | Cold Crushing Strength |
Chosun Refractories B-3 Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | <= 2.45 MPa | <= 356 psi | Cold Crushing Strength |
Chosun Refractories B-4 Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 2.45 MPa | 356 psi | Core; ASTM C365 |
3M RPF-C (0.24 g/cc) (Reinforced Polyurethane Foam) Continuous Strand Fiberglass 3M™ RPF-C (Reinforced Polyurethane Foam) is a polyurethane foam with layers of continuous strand fiberglass throughout the polyurethane matrix. The composites are 37% to 60% lighter than plywood, d.. |
|||
Compressive Strength | <= 2.45 MPa | <= 356 psi | Cold Crushing Strength |
Chosun Refractories B-5 Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |