Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Strength = 194 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 194 MPa

@Thickness 25.4 mm
28100 psi

@Thickness 1.00 in
ASTM D695
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep ..
Compressive Strength 194 MPa

@Thickness 25.4 mm
28100 psi

@Thickness 1.00 in
ASTM D695
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry)
Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr..
Compressive Strength 194 MPa
28100 psi
ASTM D695
Sumitomo Bakelite Durez® 156 Phenolic, Injection Grade
Durez 156 Black Phenolic is a two-stage, asbestos-free, heat resistant/electrical molding material. It exhibits excellent dimensional stability, high heat resistance, good molded appearance, and UL..
Compressive Strength 194 MPa
28100 psi
ASTM D695
Plenco 00732 Melamine-Phenolic, Granular, Transfer Molded
PLENCO 00732 is a melamine-phenolic copolymer molding compound, exhibiting excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 007..
Compressive Strength 194 MPa
28100 psi
ASTM D695
Plenco 3509 Phenolic, Granular, Compression Molded
PLENCO 03509 is a mineral and flock filled phenolic molding compound offering excellent electrical properties, dimensional stability, and improved heat resistance. UL recognized under component file..
Compressive Strength 194 MPa
28100 psi
ASTM D695
Plenco 7523 Phenolic, Granular, Transfer Molded
PLENCO 07523 is a woodflour and cotton flock filled novolac phenolic molding compound, formulated for high impact industrial uses. UL recognized under component file E40654.Information supplied by P..
Compressive Strength <= 194 MPa
<= 28200 psi
ASTM D695
Ensinger XP-133 Compression Molded PI Compound, 20% Carbon Fiber
The XP-130 is an amorphous high performance thermoplastic with high permanent temperature and creep resistance as well as excellent bearing and wear properties, excellent long term thermal stability..
Compressive Strength 194 MPa
28200 psi
Abatron AboCast/AboCure 4-4/50-17 Casting Epoxy for Tooling
Standard casting compound for molds or patterns of any size, that can be machined with common metal working tools, engraving and reproduction molds.Main Advantages: Easy ratiosLongest pot lifeLarges..
Compressive Strength 194 MPa
28100 psi
ASTM D695
Plenco 1510 Polyester, Granular, Transfer Molded
PLENCO 01510 is a mineral filled, pelletized polyester molding compound, which offers an excellent combination of electrical properties and dimensional stability. UL recognized under component file ..