Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Strength = 180 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 150 - 180 MPa
21800 - 26100 psi
ISO 604
Raschig Group EPOXIDUR® 3580 EP Epoxy
Glass-fiber reinforced and mineral filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties even with thin wall thicknesses and high temperatures. This prod..
Compressive Strength 140 - 180 MPa
20300 - 26100 psi
ISO 604
Bulk Molding Compounds tetra-DUR F 4401 Bulk Molding Compound
UL-licensed, general purpose productTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion prot..
Compressive Strength 160 - 180 MPa
23200 - 26100 psi
ISO 604
Bulk Molding Compounds tetra-DUR N 4111 Bulk Molding Compound
Smooth, high gloss surface. Low profile.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion..
Compressive Strength 160 - 180 MPa
23200 - 26100 psi
ISO 604
Bulk Molding Compounds tetra-DUR F 4206 Bulk Molding Compound
General purpose productTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion protection), ther..
Copyright © lookpolymers.com All Rights Reserved