Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 118 MPa | 17100 psi | |
Pyrotek NAD-11 Structural Insulation Board NAD-11 is an asbestos-free cement board with excellent electrical properties. It has a high density cement board reinforced with inorganic fibers.ApplicationsCathode support pads Platen insulation .. |
|||
Compressive Strength | 118 MPa | 17100 psi | |
Pyrotek NAD-500 Electrical Insulation Product Cement reinforcement, Inorganic fiber resinApplicationsSuperstructure support pads Bus bar insulators Pot cradle insulators Exhaust duct insulators Machined parts Wedges & shunts Point feeder gasket.. |
|||
Compressive Strength | 118 MPa | 17100 psi | |
Poco Graphite TRA Semiconductor Grade Graphite Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their .. |
|||
Compressive Strength | 118 MPa | 17100 psi | ASTM D695 |
Solvay Specialty Polymers AvaSpire® AV-848 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire® AV-848 is a high-temperature, polyaryletherketone (PAEK) that offers several key performance advantages over comparable grades of PEEK above 150°C, including better dimensional stability.. |
|||
Compressive Strength | 118 MPa | 17100 psi | ASTM D695 |
Solvay Specialty Polymers KetaSpire® KT-820 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire PEEK is produced to the highest industry standards and is characteriz.. |
|||
Compressive Strength | 118 MPa | 17100 psi | ASTM D695 |
Solvay Specialty Polymers AvaSpire® AV-848 Polyaryletherketone (PAEK) AvaSpire® AV-848 is a high-temperature, polyaryletherketone (PAEK) that offers several key performance advantages over comparable grades of PEEK above 150°C, including better dimensional stabi.. |
|||
Compressive Strength | 118 MPa | 17100 psi | ASTM D695 |
Solvay Specialty Polymers KetaSpire® KT-820 Polyetheretherketone (PEEK) KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha.. |
|||
Compressive Strength | 118 MPa | 17100 psi | ASTM D695 |
Solvay Specialty Polymers KetaSpire® KT-XXXX Polyetheretherketone (PEEK) KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha.. |
|||
Compressive Strength | 118 MPa | 17100 psi | Cold Crushing |
Sharadaa Ceramics PCF (AZS) Precast Prefired Brick Features: Manufactured under controlled conditions under refractory engineers supervision; Measured Quantity/Temperature of water, mixing by Intensive counter current mixers, Forming by Vibro Castin.. |
|||
Compressive Strength | 118 MPa | 17100 psi | ASTM D695 |
Ensinger Tecapeek® Polyetheretherketone (PEEK) Tecapeek™, made from Victrex PEEK polymer, is an excellent material for a wide spectrum of applications where thermal, chemical, and combustion properties are critical to performance.Excellent flex.. |
|||
Compressive Strength | 118 MPa @Temperature 22.8 °C |
17100 psi @Temperature 73.0 °F |
ASTM D695 |
Ensinger Tecapeek® Polyetheretherketone (PEEK) TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's excepti.. |
|||
Compressive Strength | 118 MPa | 17100 psi | Cold Crushing Strength |
Chosun Refractories AC-1 Acid-Proof and Heat-Resistant Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 118 MPa | 17100 psi | Cold Crushing Strength |
Chosun Refractories SB85S Bricks, Oxide Bonded SiC Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 118 MPa | 17100 psi | Cold Crushing Strength |
Chosun Refractories SBSN20 Nozzle Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 118 MPa | 17100 psi | |
Abatron AboCast 22-30/AboCure 50-12 Epoxy AboCast 22-30 is a black filled resin with high viscosity and a weight of 12.4 lbs/gallon. AboCure 50-12 is clear, fast converter with low viscosity and a weight of 8.2 lbs/gallon. AboCast 22-30/Abo.. |
|||
Compressive Strength | 118 MPa | 17100 psi | ASTM D695 |
ScanTube PEEK Tubing Information provided by ScanTube, Inc. |