Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 127 MPa | 18400 psi | ASTM D695 |
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK)
(Unverified Data**) Ketaspire KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provided.In.. |
|||
Compressive Strength | 127 MPa | 18400 psi | ASTM D695 |
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK) KetaSpire® KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provide.. |
|||
Compressive Strength | 127 MPa @Time 36.0 sec |
18400 psi @Time 0.0100 hour |
|
Wolf Kunststoff ZEDEX® ZX-324V1T A3H PEEK Polymer, Reinforced Main Characteristics: High resilience; High elasticity; Low permanent deformation; Stress resistant; High strength at temperatures above 140 ° CApplications: Shipbuilding; Chemical Engineering; Aut.. |
|||
Compressive Strength | <= 127 MPa | <= 18500 psi | Cold Crushing Strength |
Chosun Refractories CSN-309N Plate Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | <= 127 MPa | <= 18500 psi | Cold Crushing Strength |
Chosun Refractories CSN-309NM,Body Plate Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | <= 127 MPa | <= 18500 psi | Cold Crushing Strength |
Chosun Refractories CSN-309T Plate Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | <= 127 MPa | <= 18500 psi | Cold Crushing Strength |
Chosun Refractories CSN-322T Plate Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | <= 127 MPa | <= 18500 psi | Cold Crushing Strength |
Chosun Refractories CSN-332N Plate Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 127 MPa | 18400 psi | ASTM D695 |
Plenco 6527 Phenolic, Granular, Injection Molded PLENCO 06527 is a woodflour and mineral filled resole phenolic molding compound.Information supplied by Plenco. |