Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 123 MPa | 17800 psi | ASTM D695 |
PBI Performance Products Celazole® TL-60 Self Lubricating Melt Processable Polybenzimidazole Celazole® polybenzimidazole (PBI) resin is a unique and highly stable linear hetrocyclic polymer. PBI is characterized by high strength; excellent thermal stability, and broad chemical resistance. .. |
|||
Compressive Strength | 123 MPa | 17800 psi | ASTM D695 |
Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire PEEK is produced to the highest industry standards and is characterized by a dist.. |
|||
Compressive Strength | 123 MPa | 17800 psi | ASTM D695 |
Solvay Specialty Polymers Torlon® 4275 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4275 is a wear-resistant grade of polyamide-imide (PAI). This grade offers an excellent balance of mechanical properties and wear resistance. It offers high tensile strength and modulus with .. |
|||
Compressive Strength | 123 MPa | 17800 psi | ASTM D695 |
Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK) KetaSpire® KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire® PEEK is produced to the highest industry standards and is characterized b.. |
|||
Compressive Strength | 123 MPa | 17800 psi | ASTM D695 |
Solvay Specialty Polymers KetaSpire® KT-880FP Polyetheretherketone (PEEK) KetaSpire® KT-880FP is the high-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural color fine powder form for compression molding and other uses that can benefit from th.. |
|||
Compressive Strength | 123 MPa | 17800 psi | ASTM D695 |
Solvay Specialty Polymers Torlon® 4275 Polyamide-imide (PAI) Torlon® 4275 is a wear-resistant grade of polyamide-imide (PAI). This grade offers an excellent balance of mechanical properties and wear resistance. It offers high tensile strength and modulus w.. |
|||
Compressive Strength | 123 MPa | 17800 psi | Elastic Limit |
Wolf Kunststoff ZEDEX® ZX-324VMT A3B PEEK, Fiber Reinforced Main Characteristics: Maximum rigidity; Very good wear resistance; Low stick-slip tendency; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInfor.. |
|||
Compressive Strength | 123 MPa | 17800 psi | ASTM C-773-88 / DIN 51067T1 |
CeramTec 447 Cordierite, 2MgO•Al2O3•5SiO2 Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as c.. |