Polymer Property : Compressive Strength = 0.345 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 0.345 - 10.3 MPa
50.0 - 1500 psi
Monmouth Rubber & Plastics Bondaflexâ„¢ B33CS Sponge Neoprene Blend
Information provided by Monmouth Rubber & Plastics Corp.
Compressive Strength 0.345 MPa
50.0 psi
10% Deformation; Green
Unifrax Fiberfrax® Duraboard® LD Ceramic Fiber Board
Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard ..
Compressive Strength 0.345 MPa
50.0 psi
25% Compression, Deflection
3M Cushion-Mount™ E1715 Plus Plate Mounting Tapes with Easy Mount Adhesive
3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel..
Compressive Strength 0.345 MPa
50.0 psi
25% Compression, Deflection
3M Cushion-Mount™ 1720M Plus Plate Mounting Tape
3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr..
Compressive Strength 0.345 MPa
50.0 psi
25% Compression, Deflection
3M Cushion-Mount™ E1720 Plus Plate Mounting Tapes with Easy Mount Adhesive
3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel..