Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 0.179 MPa | 26.0 psi | 25% deformation |
Unifrax Fiberfrax® 110 Ceramic Fiber Paper 110 paper is a clay-filled, sheeted ceramic fiber paper which is denser and more rigid than other standard grade products. The rigidity is maintained even after burnout of the organic bonding agent.. |
|||
Compressive Strength | 0.179 MPa | 26.0 psi | Method B, 22 hrs @ 158°F |
Tra-Con Tra-Bond Ablebond 724-1 Polyurethane Adhesive Ablebond 724-1 premixed and frozen, polyurethane adhesive is designed for good adhesion, providing strong resilient bonds to a wide variety of substrates.Information provided by Tra-Con Inc. |
|||
Compressive Strength | 0.179 MPa | 26.0 psi | 10% Compression, Deflection |
3M Cushion-Mount™ E1515 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Compressive Strength | 0.179 MPa | 26.0 psi | 10% Compression, Deflection |
3M Cushion-Mount™ E1520 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |