Mechanical Properties Metric English Comments
Tensile Strength 6.72 MPa
975 psi
Silicone Property; ASTM D412
Arlon 55590R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: Style 162 FiberglassThis data represents typical values for the production material. The data should not be us..
Tensile Strength 6.72 MPa
975 psi
Silicone Property; ASTM D412
Arlon 55591R062 0.062" (1.57 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave 1: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene Product Use: Electrical insula..
Tensile Strength 6.72 MPa
975 psi
Silicone Property; ASTM D412
Arlon 48B12R005 0.005" (0.127 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 1080 FiberglassThis data represents typical values for the production material. The data should not be used..
Tensile Strength 6.72 MPa
975 psi
Silicone Property; ASTM D412
Arlon 48B10R005 0.005" (0.127 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1080 FiberglassThis data represents typical values for the production material. The data should not be us..