Mechanical Properties Metric English Comments
Tensile Strength 96.5 MPa
14000 psi
ASTM D638
Quadrant EPP Ketron® GF30 PEEK, Extruded 30% Glass-Reinforced Polyetherether Ketone (ASTM Product Data Sheet)
Tensile Strength 96.5 MPa
14000 psi
ASTM D638
Solvay Specialty Polymers KetaSpire® KT-820FP Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-820FP is the low-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color fine powder form suitable for compression molding. KetaSpire PEEK is produced to the ..
Tensile Strength 96.5 MPa
14000 psi
51 mm/min; ASTM D638
Solvay Specialty Polymers KetaSpire® KT-850 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-850 is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color pellet form. KetaSpire PEEK is produced to the highest industry standards and ..
Tensile Strength 96.5 MPa
14000 psi
ASTM D638
Solvay Specialty Polymers KetaSpire® KT-850P Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-850P is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire PEEK is produced to the highest industry standa..
Tensile Strength 96.5 MPa
14000 psi
ASTM D638
Quadrant EPP Ketron® GF30 LSG PEEK, Extruded 30% Glass-Reinforced Polyetherether Ketone (ASTM Product Data Sheet)
Tensile Strength 96.5 MPa
14000 psi
ASTM D638
Quadrant EPP Semitron® ESd 490HR Static dissipative PEEK for use in test fixtures. Non-sloughing and low moisture absorption. (ASTM Product Data Sheet)
Tensile Strength 96.5 MPa
14000 psi
ASTM D638
Solvay Specialty Polymers Udel® GF-120 Polysulfone (PSU)  (Unverified Data**)
Udel GF-120, resin is a 20% glass fiber reinforced polysulfone compound. Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical resi..
Tensile Strength 96.5 MPa
14000 psi
ASTM D638
Solvay Specialty Polymers KetaSpire® KT-820FP Polyetheretherketone (PEEK)
KetaSpire® KT-820FP is the low-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color fine powder form suitable for compression molding. KetaSpire® PEEK is produced..
Tensile Strength 96.5 MPa
14000 psi
50 mm/min; ASTM D638
Solvay Specialty Polymers KetaSpire® KT-850 Polyetheretherketone (PEEK)
KetaSpire® KT-850 is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color pellet form. KetaSpire® PEEK is produced to the highest industry standa..
Tensile Strength 96.5 MPa
14000 psi
ASTM D638
Solvay Specialty Polymers KetaSpire® KT-850P Polyetheretherketone (PEEK)
KetaSpire® KT-850P is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire® PEEK is produced to the highest industr..
Tensile Strength 96.5 MPa
14000 psi
ASTM D638
Solvay Specialty Polymers Udel® GF-120 Polysulfone (PSU), Glass Fiber
Udel® GF-120, resin is a 20% glass fiber reinforced polysulfone compound. Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical ..
Tensile Strength 96.5 MPa
14000 psi
ASTM D638
Teknor Apex Chemlon® 104-13 GH Nylon 66, 13% Glass Fiber Reinforced
Notes: Impact Modified; Reinforced with 13% Glass Fibers; Synergistic compound exhibiting impact strength and dimensional stability Features: Good Dimensional stability; Good Processability; Heat St..
Tensile Strength 96.5 MPa
14000 psi
ASTM D638
Ensinger XP-132 Compression Molded PI Compound, 15% Graphite Filled
The XP-130 is an amorphous high performance thermoplastic with high permanent temperature and creep resistance as well as excellent bearing and wear properties, excellent long term thermal stability..
Tensile Strength 96.5 MPa
14000 psi
ASTM D882
Arlon 25FR Low-Cost Ceramic Hydrocarbon
High Frequency, Low Loss Thermoset Laminate and Prepreg for Double-sided, Multilayer and Mixed Dielectric Printed Circuit BoardsLow loss ceramic-filled thermoset resinTight dielectric tolerance cont..
Tensile Strength 96.5 MPa
14000 psi
ASTM D638
Aaron Industries AAROPRENE® G/MFN 6602 Glass and Mineral Filled Nylon 6/6
AAROPRENE® GFN & MFN 6600 Series Reinforced CompoundsColor may be specified.
Tensile Strength 96.5 MPa
14000 psi
ASTM D638
Quantum PEEK