Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength = 96.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 96.0 MPa

@Thickness 0.0250 mm
13900 psi

@Thickness 0.000984 in
ASTM D882-02
NeXolve Novastrat® 400 Polyimide
Colorless polyimide with high temperature stability.NeXolve Novastrat® 400 is a colorless polyimide with a higher temperature stability than NeXolve’s LaRC™CP1, exhibiting a glass transition temp..
Tensile Strength 96.0 MPa
13900 psi
ASTM D638
Solvay Specialty Polymers KetaSpire® KT-820P Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-820P is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire PEEK is produced to the highest industry standards and is ..
Tensile Strength 96.0 MPa
13900 psi
ASTM D638
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and pro..
Tensile Strength 96.0 MPa
13900 psi
ASTM D638
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insulation..
Tensile Strength 96.0 MPa
13900 psi
ASTM D638
Solvay Specialty Polymers KetaSpire® KT-820P Polyetheretherketone (PEEK)
KetaSpire® KT-820P is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire® PEEK is produced to the highest industry standards..
Tensile Strength 96.0 MPa
13900 psi
ASTM D638
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK)
KetaSpire® KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insula..
Tensile Strength 96.0 MPa
13900 psi
ASTM D638
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)
KetaSpire® KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and..
Tensile Strength 96.0 MPa
13900 psi
5 mm/min; ISO 527-1
Sax Polymers SAXAMID 136F6Q32 Nylon 6, 30% Glass Fiber
SAXAMID 136F6Q32 is a high-impact-modified polyamide 6 injection-molding-grade reinforced with 30% glass fibers . Beside the high impact strength at low temperatures this grade shows very good proce..
Tensile Strength 96.0 MPa
13900 psi
ASTM D638
Lubrizol ESTALOC® 59600 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane
Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas, Europe, Middle East, Africa, India and AsiaInformation pro..
Copyright © lookpolymers.com All Rights Reserved