Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 0.0683 MPa @Thickness 3.00 mm |
9.90 psi @Thickness 0.118 in |
ASTM D412 |
Parker Chomerics SOFT-SHIELD® 4850-STRIP Low-Closure Force Strip Gasket Description: SOFT-SHIELD® 4850-STRIP multi-planar, Z-axis conductive strip gaskets are a new, convenient form of the successful 4850 EMI sheet gasket. These strip gaskets provide EMI shielding in t.. |
|||
Tensile Strength | 0.0683 MPa | 9.90 psi | |
Parker Chomerics SOFT-SHIELD® 4800 Multi-planar EMI Gasket Description: SOFT-SHIELD® 4800 Multi-planar conductive Z axis foam EMI gaskets is soft foam based EMI shielding technology. The integration of electrically conductive fibers into low density foam p.. |
|||
Tensile Strength | 0.0683 MPa @Thickness 3.00 mm |
9.90 psi @Thickness 0.118 in |
ASTM D412 |
Parker Chomerics SOFT-SHIELD® 4850 Multi-planar EMI Gasket Description: SOFT-SHIELD® 4850 represents the latest advancement in EMI shielding gaskets based on Multi-planar, Z-axis conductive foam technology. SS4850 is based on the unique integration of elec.. |