Mechanical Properties Metric English Comments
Tensile Strength 9.65 MPa
1400 psi
ASTM D638
S&E Specialty Polymers GTP09005 PVC
A proprietary, low gravity, non-halogen based flame retardant thermoplastic polyolefin designed for extrusion in wire and cable applications.Information provided by S&E Specialty Polymers
Tensile Strength 9.65 MPa
1400 psi
ASTM D638
S&E Specialty Polymers GTP09008-1 PVC
Non-halogen flame retardant TPO for wire and cable extrusion.Information provided by S&E Specialty Polymers
Tensile Strength 9.65 MPa
1400 psi
ASTM D412
S&E Specialty Polymers TufTech™ G-3570 PVC Compound
Application: A PVC compound designed for work boot and boat shoe soling applications.Information provided by S&E Specialty Polymers
Tensile Strength 9.65 MPa

@Strain 100 %
1400 psi

@Strain 100 %
510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible A8500 Polyvinyl Chloride, Flexible (PVC, Flexible)
Recommended for interior applications.Information provided by PolyOne
Tensile Strength 9.65 MPa

@Strain 100 %
1400 psi

@Strain 100 %
510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible A8501 Polyvinyl Chloride, Flexible (PVC, Flexible)
Recommended for interior applications.Information provided by PolyOne
Tensile Strength 9.65 MPa

@Strain 100 %
1400 psi

@Strain 100 %
510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible B83UB Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength 9.65 MPa

@Strain 100 %
1400 psi

@Strain 100 %
510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible D8500 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength 9.65 MPa

@Strain 100 %
1400 psi

@Strain 100 %
510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible D9000 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength 9.65 MPa

@Strain 100 %
1400 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible R336AE Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength 9.65 MPa
1400 psi
Typical
Garlock 4160 Natural Sheet Rubber
Excellent general purpose gasket materials for air, hot and cold water, saturated steam and exterior service.Red, smooth finishInformation provided by Garlock Rubber Technologies
Tensile Strength 9.65 MPa
1400 psi
across grain; ASTM F152
Garlock 706 Compressed Inorganic Fiber Gasketing, Nitrile Binder
Inorganic fibers with a nitrile binder.Inorganic, asbestos-free fibers offer superior performance in saturated and superheated steamThermally stable fibers retain effective seal even during thermal ..
Tensile Strength 9.65 MPa
1400 psi
Machine Direction; Injection molded sample tested at 10 in/min with Die D; ASTM D412
Kraton® D2104 DI-N (SBS) Compound
Description: Kraton D2104 DI-N is an easy processing, general purpose material designed for a wide variety of applications. It is supplied from North America in the physical form identified: D2104 D..
Tensile Strength 9.65 MPa
1400 psi
Silicone Property; ASTM D412
Arlon R39118R037L 0.037" (0.940 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyester Release Liner Transfer Pressure Sensitive Adhesive: Silicone PSASide 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Cured Silicone Rubber..
Tensile Strength 9.65 MPa
1400 psi
Silicone Property; ASTM D412
Arlon T4020-R002 0.020" Cured, Fusible Silicone Rubber with Fiberglass Substrate
0.5 inch wide, 20 mil thick, red, rectangular cross-section, fusible silicone tape.Design/Construction:Side 1: Cured Fusible Silicone RubberSubstrate: 15% Sinusoidal FiberglassSide 2: Cured Fusibl..
Tensile Strength 9.65 MPa
1400 psi
AlphaGary Garathane™ X 96-322 A Polyurethane based compound
Abrasion & Slip Resistant
Tensile Strength 9.65 MPa
1400 psi
AlphaGary Garaflex™ O 9939NA Olefinic Thermoplastic Elastomer
Garaflex™ O is a flame retarded, olefinic thermoplastic elastomer105°C rated flame retardant olefinic TPE for flat ribbon cable and heat tracing cable
Copyright © lookpolymers.com All Rights Reserved