Mechanical Properties Metric English Comments
Tensile Strength 54.0 MPa
7830 psi
Perstorp Compounds Akestra™ 90 Thermoplastic Copolyester
Akestra™ is a thermoplastic with a sparkling glass-like appearance. It can be used as a polystyrene alternative for heat resistant thin wall containers, a polycarbonate alternative for durable “di..
Tensile Strength 54.0 MPa
7830 psi
ASTM D638
Kolon KOCETAL® K300BK Black Colored Grade Acetal Resin
Colored, general purpose injection molding grade. Applications: General injection molding products.Information provided by API-Kolon.
Tensile Strength 54.0 MPa
7830 psi
ASTM D638
Kolon KOCETAL® K300HRD Wear Modified Acetal Resin
Improved weather resistant grade suitable for out door use. Applications: Weather resistant products. Information provided by API-Kolon.
Tensile Strength 54.0 MPa
7830 psi
ASTM D638
Kolon KOCETAL® LF301 Wear Modified Acetal Resin
Special polymer added, improved wear property. Applications: Products for low noise and precision gear. Information provided by API-Kolon.
Tensile Strength 54.0 MPa
7830 psi
ASTM D638
Kolon KOCETAL® VT301 Anti-Static Grade Acetal Resin
Improved antistatic effects. Applications: Products for avoiding electric contamination. Information provided by API-Kolon.
Tensile Strength 54.0 MPa
7830 psi
ASTM D638
Kolon KOCETAL® WR301 Wear Modified Acetal Resin
Improved weather resistant grade suitable for out door use. Applications: Weather resistant products. Information provided by API-Kolon.
Tensile Strength 54.0 MPa
7830 psi
ASTM D638
Kolon KOCETAL® WR301LO Wear Modified Acetal Resin
Improved weather resistance and low odor of FA. Applications: Weather resistant products at closed space. Information provided by API-Kolon.
Tensile Strength 54.0 MPa
7830 psi
ASTM D638
Kolon SPESIN® KP270 General Purpose PBT Base Resin
Excellent extrudabilityApplications: CablesInformation provided by API-Kolon.
Tensile Strength 54.0 MPa
7830 psi
Weld; ASTM D638
Kuraray Genestarâ„¢ GN2330 Nylon, 33% Glass Filled
Standard V-0 Grade. Features a balance of mechanical strength, mold-ability, and dimensional stability. Well suited for a wide range of electrical and electronic components.
Tensile Strength 54.0 MPa

@Strain 20.0 %,
Temperature 40.0 °C
7830 psi

@Strain 20.0 %,
Temperature 104 °F
50 mm/min; ISO 527-2
BASF Elastollan R 2000 20% Glass Filled TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan..
Copyright © lookpolymers.com All Rights Reserved