Polymer Property : Tensile Strength = 750 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 5.17 MPa

@Strain 100 %
750 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible MG23B Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength 5.17 MPa

@Strain 100 %
750 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ HC 2155 Polyvinyl Chloride, Flexible (PVC, Flexible)
Geon HC 2155 is a 55 Shore A non-phthalate flexible vinyl compound made from FDA sanctioned ingredients. HC 2155 can be used for extrusion and injection molding healthcare applications.NOTE: All ing..
Tensile Strength 5.17 MPa

@Strain 100 %
750 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ HC 2155G Polyvinyl Chloride, Flexible (PVC, Flexible)
Geon HC 2155G is a 55 Shore A non-phthalate, gamma-stable flexible vinyl compound made from FDA sanctioned ingredients. HC 2155G can be used for extrusion and injection molding healthcare applicatio..
Tensile Strength 5.17 MPa
750 psi
Side 2; ASTM D412
Arlon 18646B026 0.026" (0.66 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: 11523 Style FiberglassSide 2: Uncured Silicone RubberInterleave: PolyethyleneThis data represents typical values for the production materi..
Tensile Strength 5.17 MPa
750 psi
Silicone Property; ASTM D412
Arlon CP-PC-2951 Silicone Compound
This data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Tensile Strength 5.17 MPa
750 psi
Silicone Property; ASTM D412
Arlon P29514R015 0.0165" (0.419 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Self-Fusing Silicone RubberSubstrate: 7727 Style FiberglassProduct Advatages:Flexibility: Silicone rubber resists damage due to vibration, frame movement under loa..
Tensile Strength 5.17 MPa
750 psi
Silicone Property; ASTM D412
Arlon P29514R020 0.0205" (0.521 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Self-Fusing Silicone RubberSubstrate: 7727 Style FiberglassAppearance: Red silicone rubber on fiberglass fabric.This data represents typical values for the product..
Tensile Strength 5.17 MPa
750 psi
Silicone Property; ASTM D412
Arlon P29514R020P 0.0205" (0.521 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: Polyethylene Side 1: Cured Self-Fusing Silicone RubberSubstrate: 7727 Style FiberglassThis data represents typical values for the production material. The data should..
Tensile Strength 5.17 MPa
750 psi
Silicone Property
Arlon R30370A008 0.008" Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 0.001" FEP FilmSide 1: Unsupported/Uncured Silicone RubberSubstrate: 0.003" PTFE coated FiberglassThis data represents typical values for the production material a..
Tensile Strength 5.17 MPa
750 psi
Silicone Property; ASTM D412
Arlon R38026B017 0.017" (0.432 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 1165 FiberglassSide 2: Uncured Silicone Rubber Interleave: LDPEThis data represents typical values for the production material. The..
Tensile Strength 5.17 MPa
750 psi
Silicone Property; ASTM D412
Arlon Thermabond® 48781A008 0.008" (0.203 mm) Uncured Silicone Rubber with Fiberglass Substrate
Description: Generation II Thermabond® NP electrically insulating electronic adhesive. Bonds without primer.Design/Construction: Liner 1: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style..
Tensile Strength 5.17 MPa
750 psi
Silicone Property; ASTM D412
Arlon Thermabond® R36200A008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated Fiberglass Appearance: Blue silicone gumThis data represents typical values for the production material. The d..
Tensile Strength 5.17 MPa
750 psi
Silicone Property; ASTM D412
Arlon Thermabond® R36211A008 0.008" (0.203 mm) Uncured Silicone Rubber with Fiberglass Substrate
Description: Generation II Thermabond® NP electrically insulating electronic adhesive. Bonds without primerDesign/Construction: Liner 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: St..
Tensile Strength 5.17 MPa
750 psi
Silicone Property
Arlon R30370A015 0.015" Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 0.001" FEP FilmSide 1: Unsupported/Uncured Silicone RubberSubstrate: 0.003" PTFE coated FiberglassThis data represents typical values for the production material a..
Tensile Strength >= 5.17 MPa
>= 750 psi
Compound Property
Arlon R33991R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place ..