Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 50.3 MPa
7300 psi
ASTM D-638
Plaskolite Optix® CA - 42 FDA General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
Tensile Strength 50.3 MPa
7300 psi
ASTM D-638
Plaskolite Optix® CA - 42 General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
Tensile Strength 50.3 MPa
7300 psi
ASTM D-638
Plaskolite Optix® CA - 927 High Impact Grade Acrylic Resin
OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc.
Tensile Strength 50.3 MPa
7300 psi
ASTM D638
Plaskolite Optix® CA-990 Impact Modified Acrylic Resin
Injection Molding and Extrusion Grade. Excellent surface gloss.
Tensile Strength 50.3 MPa
7300 psi
ASTM D-638
Plaskolite Optix® CP - 927 High Impact Grade Acrylic Resin
OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc.
Tensile Strength 50.3 MPa
7300 psi
ASTM D-638
Plaskolite West Optix® CA - 927 High Impact Acrylic Resin
Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g..
Tensile Strength 50.3 MPa
7300 psi
ASTM D638
Plaskolite West Optix® CA-990 Impact Modified Acrylic Resin
Injection Molding and Extrusion Grade. Excellent surface gloss.
Tensile Strength 50.3 MPa
7300 psi
ASTM D-638
Plaskolite West Optix® CP - 927 G High Impact Acrylic Resin
Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g..
Tensile Strength 50.3 MPa
7300 psi
ASTM D-638
Plaskolite West Optix® CP - 927 High Impact Acrylic Resin
Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g..
Tensile Strength 50.3 MPa
7300 psi
ASTM D-638
Plaskolite Optix® CP - 927 G High Impact Grade Acrylic Resin
OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc.
Tensile Strength 50.3 MPa
7300 psi
ASTM D-638
Plaskolite West Optix® CA - 42 FDA General Purpose Acrylic Resin
Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av..
Tensile Strength 50.3 MPa
7300 psi
ASTM D-638
Plaskolite West Optix® CA - 42 General Purpose Acrylic Resin
Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av..
Tensile Strength 50.3 MPa
7300 psi
ASTM D638
Techmer ES Elastoblend® PA6 IM HS L
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedInformation provided by TP Composites, Inc.
Tensile Strength 50.3 MPa
7300 psi
ASTM D412/D638
Lubrizol ESTANE® 5707 Ester Based Thermoplastic Polyurethane
Features: Very high tensile strength, excellent low temperature flexibility and superior abrasion and cut resistance. It is processed by means of solution coating, extrusion and melt coating.Uses: S..
Tensile Strength 50.3 MPa
7300 psi
ASTM D412/D638
Lubrizol ESTANE® 5719 Ester Based Thermoplastic Polyurethane
Features: High tensile strength, low temperature flexibility, and high adhesion to various substrates such as PET, PVC, and various fabrics.Uses: Fabric coating and audio tape binder, inks and solut..
Copyright © lookpolymers.com All Rights Reserved