Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength = 7.86 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 7.86 MPa

@Strain 100 %
1140 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ HC 2180 Polyvinyl Chloride, Flexible (PVC, Flexible)
Geon HC 2180 is a 80 Shore A non-phthalate flexible vinyl compound made from FDA sanctioned ingredients. HC 2180 can be used for extrusion and injection molding healthcare applications.NOTE: All ing..
Tensile Strength 7.86 MPa

@Strain 100 %
1140 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ HC 2180G Polyvinyl Chloride, Flexible (PVC, Flexible)
Geon HC 2180G is a 80 Shore A non-phthalate, gamma-stable flexible vinyl compound made from FDA sanctioned ingredients. HC 2180G can be used for extrusion and injection molding healthcare applicatio..
Tensile Strength 7.86 MPa

@Strain 100 %
1140 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ HC 3180G Polyvinyl Chloride, Flexible (PVC, Flexible)
Geon HC 3180G is a non-phthalate, gamma-stable flexible vinyl compound made from FDA sanctioned ingredients. HC 3180G can be used for extrusion and injection molding healthcare applications. This pr..
Tensile Strength 7.86 MPa

@Strain 100 %
1140 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible XV3856 Polyvinyl Chloride, Flexible (PVC, Flexible)
All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high ..
Tensile Strength 7.86 MPa
1140 psi
Silicone Property; ASTM D412
Arlon 56606R026 0.027" Cured/Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 1564 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production materia..
Tensile Strength 7.86 MPa
1140 psi
Silicone Property; ASTM D412
Arlon P30670R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Uncured Silicone Rubber Substrate: Style 1165 FiberglassAppearance: Red silicone gum on fiberglass with polymer release linersThis data represents typical values for the..
Tensile Strength 7.86 MPa
1140 psi
Silicone Property; ASTM D412
Arlon 44602W020W 0.020" (0.508 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 1165 FiberglassProduct is designed to meet the FAR 25.853 App.F, P.1,.Aii flame resistance requirements b..
Copyright © lookpolymers.com All Rights Reserved