Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 48.0 MPa @Thickness 0.0440 mm |
6960 psi @Thickness 0.00173 in |
ASTM D882-02 |
NeXolve White Optionox® Polyimide Film Highly UV durable with excellent weatherability and stability to ozone.Optinox® films and coatings are highly UV durable and exhibit excellent weathering durability, including very high stability .. |
|||
Tensile Strength | 48.0 MPa | 6960 psi | ISO 527-1 |
Sax Polymers SAXLAC 120U Acrylonitrile Butadiene Styrene Saxalac 120U is an UV protected easy flowing ABS injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Mechanical property data tested.. |
|||
Tensile Strength | >= 48.0 MPa | >= 6960 psi | ISO 37 |
Austin Novel Materials Texalan® 264D Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech |
|||
Tensile Strength | >= 48.0 MPa | >= 6960 psi | ISO 37 |
Austin Novel Materials Texalan® 764D PCL TPU Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech |
|||
Tensile Strength | >= 48.0 MPa | >= 6960 psi | ISO 37 |
Austin Novel Materials Texalan® 598A Polyether-based TPU Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech |
|||
Tensile Strength | 48.0 MPa | 6960 psi | 5 mm/min; ISO 527-2 |
CENTROPLAST CENTRODAL MD Polyoxymethylene, Magnetically Detectable During the modification with POM MD, metal fillings are added to the basic polyoxymethylene, which allows the plastic to be detectable. The excellent machinability, tenacity and dimensional stabilit.. |