Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 44.1 MPa | 6400 psi | ASTM D412 |
Kolon ELLAS K-429A Ester Based Thermoplastic Polyurethane ApplicationsIndustry PartsOutsole of Soccer ShoeHighly Pressurized Hose Information provided by API-Kolon. |
|||
Tensile Strength | 44.1 MPa | 6400 psi | ASTM D412 |
Kolon ELLAS K-480A Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionCompoundingIndustry PartsParts for Automobile/Mobile phoneAcetal Compound Information provided by API-Kolon. |
|||
Tensile Strength | 44.1 MPa | 6400 psi | ASTM D412 |
Kolon ELLAS K-490AB Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionFilm/SeatBlown filmIndustry Parts Information provided by API-Kolon. |
|||
Tensile Strength | 44.1 MPa | 6400 psi | ASTM D412 |
Kolon ELLAS K-585A Caprolactone Based Thermoplastic Polyurethane ApplicationsInjectionIndustry Parts Information provided by API-Kolon. |
|||
Tensile Strength | 44.1 MPa | 6400 psi | ASTM D638 |
GRECO ISOPAK 569 ABS Resin Extrusion GradeInformation provided by Greater Eastern Resins Industrial Co., Ltd. |
|||
Tensile Strength | 44.1 MPa | 6400 psi | 50 mm/min; ISO 527-1,-2 |
Gromax BTE35-DN00N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Tensile Strength | >= 44.1 MPa | >= 6400 psi | ASTM D 638 |
Karina E 786-10/332-IS-RG Compound PVC White White rigid for spiral hoses (non-toxic)Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | 44.1 MPa | 6400 psi | 50 mm/min; ISO 527-1,-2 |
Gromax ATE70-FN00N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Tensile Strength | 44.1 MPa | 6400 psi | |
Taiwan Sheen Soon Sheenthane® A9513H TPU for Ink Thermoplastic polyurethane elastomer for inkAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen printing, and spray applicati.. |
|||
Tensile Strength | 44.1 MPa | 6400 psi | |
Taiwan Sheen Soon Sheenthane® A9600R Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Tensile Strength | 44.1 MPa | 6400 psi | |
Taiwan Sheen Soon Sheenthane® D6320E Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Tensile Strength | 44.1 MPa | 6400 psi | |
Taiwan Sheen Soon Sheenthane® A9720 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Tensile Strength | 44.1 MPa | 6400 psi | |
Taiwan Sheen Soon Sheenthane® A9720E Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Tensile Strength | 44.1 MPa | 6400 psi | ASTM D638 |
Samyang Trimma® SD6320 PMMA, Translucent High scratch resistance; stability against weak acids, strong acids, weak alkalis and inorganic salts.Applications: Laptop, Monitor Front Cover - for high flow, high gloss and high hardnessInformat.. |
|||
Tensile Strength | 44.1 MPa @Temperature 23.0 °C |
6400 psi @Temperature 73.4 °F |
EN ISO 527 |
Ensinger TECASINT 3062 Polyimide, Shiny Black, 15% Graphite, 10% PTFE (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Tensile Strength | 44.1 MPa | 6400 psi | ASTM D638 |
Americas Styrenics STYRON® 610 High Heat Crystal Polystyrene Product CharacteristicsAdditive freeTypical ApplicationsFoamsFilms/opticalCarrier resinSpecialty blendingInformation provided by AmericasStyrenics LLC. |
|||
Tensile Strength | 44.1 - 57.9 MPa | 6400 - 8400 psi | |
Bulk Molding Compounds BMC A20-(a) High Strength Grade Molding Compound BMC A20 is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC A20 is well suited for injection, transfer or compression molding o.. |